anyone here have some experience with hot rolling with high reduction %?

I have been hot rolling some magnesium sheets (@ 400 celcius), with no problems at low reduction %s, however i am tryting to go up to 50% reduction per pass, but am facing some difficulties, mainly that the rollers aren't biting my sample. and instead the samples is sort of just hanging around at the entrance of the roller even when im trying to push it in. How is this issue solved usually in industry when hot rolling sheets?

thank you.

submitted by /u/tiredscientist123
[link] [comments]

from The ME Hang Out https://ift.tt/2Yb6Khy https://ift.tt/eA8V8J